Choosing a process

SLS vs SLA vs FFF

Three industrial 3D printing processes, side by side: materials, part size, strength, surface finish and what each one is best for. All three are made in our Milton Keynes facility.

At a glance

Process comparison

Property SLSSelective Laser Sintering SLAStereolithography FFFFused Filament Fabrication
How it worksA laser fuses nylon powder, layer by layerA UV laser cures liquid resin, layer by layerReinforced filament is laid down, layer by layer
MaterialPA12 nylonSomos® WaterShed resinDYNAMIDE® CF and GF (fibre-reinforced polyamide)
ColourBlackTransparentBlack and grey
Max part size400 x 400 x 540 mm450 x 450 x 400 mm500 x 340 x 485 mm (LOOP PRO X+ TURBO)
Layer thickness0.1 mm0.1 mm0.1 to 0.263 mm
Support structuresNone neededNeeded, removed after printingBreakaway support, removed after printing
Tensile strength48.2 MPa50.4 MPaCF 105 MPa, GF 85 MPa
Heat deflection (0.45 MPa)147 °C–CF 214 °C, GF 190 °C
Surface off the machineSlightly grainy, matteVery smoothVisible layer lines
Vapour smoothingYesNoYes, DYNAMIDE® GF
Best forFunctional parts, complex shapes, production runsFine detail, clear parts, investment casting patternsStrong, stiff parts, jigs and fixtures, large parts

Strength and temperature values are typical datasheet values in the X-Y direction, indicative only. Real parts depend on geometry, orientation and finishing.

Quick guide

Which one should I choose?

Choose SLS if…

  • You need strong, functional nylon parts
  • Your part has complex or internal features
  • You need tens or hundreds of parts
More about SLS

Choose SLA if…

  • You need fine detail and a smooth surface
  • You need clear, see-through parts
  • You will paint or finish the part to a high standard
More about SLA

Choose FFF if…

  • You need maximum stiffness and strength
  • You need parts that work at high temperatures
  • You need large parts, jigs or fixtures
More about FFF
Finishing

Finishes by process

FinishWhat it doesAvailable for
StandardDe-powdering and bead blasting (SLS), support removal (SLA, FFF), inspectionSLS, SLA, FFF
Sanding, painting, varnishingA very high standard of cosmetic finishSLA
DyeingBlack onlySLS
Vapour smoothingSealed against liquids and gases, injection-moulding-quality surfaceSLS, FFF (DYNAMIDE® GF)
FAQs

Choosing a process

Which process gives the strongest parts?

FFF in DYNAMIDE® CF has the highest tensile strength we offer (105 MPa in X-Y). For complex shapes that must be strong in every direction, SLS PA12 is often the better choice because it needs no supports.

Which process gives the smoothest surface?

SLA has the smoothest surface straight off the machine. SLS and DYNAMIDE® GF parts can be vapour smoothed for a sealed, injection-moulding-quality finish.

Can I get transparent parts?

Yes, with SLA in Somos® WaterShed, an optically clear resin.

Which process is best for production runs?

SLS: we nest many parts in each build and need no supports, so it scales well from one-offs to repeat production.

Still not sure which process?

Upload your file for an instant price, or describe your part and our engineers will recommend the right process.